Eryone
PLA Filament - 1.75mm±0.03mm (1kg)
PLA Filament - 1.75mm±0.03mm (1kg)
SKU:B0101030
26 in stock
Couldn't load pickup availability
Technical Specification
Print Any Model You Want with ERYONE PLA Filament.
Material: PLA
Length: 340m
Diameter: 1.75mm±0.03mm
Printing temperature: 190-220℃
Heated bed temperature: 55-70°C
Recommended Printing Temperature: 210-220℃
Recommended Print Speed: 30-100m
|
|
|
|
---|---|---|---|
Neat WindingThe PLA threads are arranged neatly, without the risk of knotting that makes printing more comfortable. |
Premium QualityMaterial wire diameter 1.75mm±0.03mm, ensure smooth output line, vacuum packaging without bubbles, does not block nozzle, make the printing more smooth. |
Good AdhesionExcellent first layer adhesion to reduce warpage, shrinkage, curl and print failure. |
Good Layer BondingGood layer bonding strength makes the printing parts stronger. The printed model has a smooth surface. |
The Difference between White&Gray&Black
Showcase:
FAQ
1.Q: Can PLA be used to print tableware?
A: Not recommended. Although PLA is degradable, food-grade raw material, the PLA with toner is non-food grade. If you really want to print a set of tableware, transparent PLA is suggested.
2.Q: The nozzle is clogged by PLA, and how can I solve it?
A: Inconstant filament diameter, the lower nozzle temperature and frequent replacement with different kinds of filaments will lead to this problem. So, before you get started, clean the nozzle and turn up the temperature to a proper value.
3.Q: My prints have web-like strings (stringing) issues. How can I troubleshoot it?
A: Too high temperature makes the PLA filament melt and flow so fast. Please turn the temperature down to a proper value.
The retracting parameters are improper, so adjust the retracting length and speed.
4.Q: There are too much melted filament around the nozzle. What should I do?
A: This problem can be attributed to over-high temperature, low printing speed, and in the slice software, the nozzle diameter doesn't match with the extrusion output.
5.Q: The PLA filament was perfect when I opened the package. After several times of intermittent printing, my PLA filament snaps by accident during printing. Why?
A: Normally, the PLA filament in the printing process will not snap by itself. However, after being affected by moisture, the degradable material PLA will be more brittle and easier to break, so you should pay attention to dampproof.
6.Q: The surface of my print isn't very smooth, and the extruded filament has inconsistent diameters. Why?
A: The printing temperature is too high or too low. The temperature doesn't match well with the printing speed. You need to adjust the printing speed or temperature.
7.Q: Why my PLA-printed objects don't stick to the heated bed? How do I solve?
A: The distance between the nozzle and the bed is too far. Make sure your heated bed is leveled and it's clean. Then judge if the printing temperature and heated bed temperature are too low, and our customers should adjust them to correct ranges.